Domestik gwo avyon 8 pousan sèvi ak alyaj Titàn

Mar 03, 2022

Ranplase gwo avyon domestik akalyaj Titàn

An 2006, Konsèy Eta a te apwouve etablisman yon komite demonstrasyon gwo avyon konplo. Cao Chunxiao se sèl manm ki angaje nan rechèch materyèl avyasyon. Apre lansman pwojè a, Cao Chunxiao te sèvi kòm yon manm nan komite konsiltatif ekspè ak vwayaje nan tout peyi a. Gwo pwojè avyon an kouvri avyon sivil ak militè, ak kòd avyon sivil la se C919.

The less weight an airplane has, the better. The weight of the airplane itself is a percentage of its total take-off weight, which is called the "structural weight coefficient of the airplane". In the past 70 years, no aircraft has had a structural weight factor of less than 27 percent , which is due to the performance of large components and the manufacturing capacity of large components. Titanium material becomes the key. Titàn alyajmateryèl ak teknoloji forge ka diminye pwa estriktirèl avyon an ak amelyore compétitivité li yo.

Domestic large aircraft 8% use titanium alloy

Today, the more economically demanding C919 uses 8 percent titanium, comparable to 7.5 percent of the Boeing 777 in the U.S. Large aircraft can not be manufactured without large forgings which require high technology. In the column "Academician's Introduction", Cao Chunxiao shows Titàn forging joint for C919, named TC4, weighing 600 kg. To make similar forgings, China has built the world's largest 80,000-ton hydraulic press.

In November 2015, C919 with China's independent intellectual property rights was officially unveiled worldwide in Shanghai. Cao Chunxiao was thrilled at the scene and his dream of more than forty years came true at last.

Sou 5 me 2017, avyon an C919 te fè premye vòl siksè li nan Shanghai. Nan mwa mas 2021, C919 te pran premye lòd la. Nan kòmansman 2022, C919 la te pran 815 lòd.