BT6 Titanium Plak

BT6 Titanium Plak

Titanium fèy BT6
BT6 (VT6) titanium fèy
Gr5 titanium Ti-6AL-4V plak
Bt6 Titanium Plak pou vann
Voye rechèch
Chat kounye a
Dekri teren

 

Pwodwi Entwodiksyon

1. BT6 titanium plakse yon fèy metal Larisi-klas, ki se youn nan plak yo ki pi lajman itilize titanium, ki gen fòs segondè ak bon rezistans korozyon.

2. Titanium alyaj fèy BT6 gwosè ki disponib ak estanda

OD: 0.5 ~ 200mm oswa gwosè kliyan an

Estanda: ΓOCT23755-87 ΓOCT22178-90 DIN17860-1990

3. Pwopriyete titanium fèy BT6

Li te gen Al la ak V eleman, BT6 (Al 5.3 ~ 6.8, V 3.5 ~ 5.3) ki gen gwo fòs tensi, ak plis Zr ak Sileman vs Grade5 titanium alyaj.

BT6 (VT6) titanium sheet
titanium alloy sheet BT6

4. Konpozisyon chimik yo nan plak la BT6 (VT6) plak Titàn

KlasKonpozisyon chimik (fraksyon mas) (%) pa pi gran pase (eksepte pou valè ranje espesifye)

TibèkilalCrMouvmanSnMnVFesizoZrCNHOsòm lòt eleman yo
vt6Baz5.3 ~ 6.83.5-5.30.60.150.30.10.050.0150.20.3
BT1-0Baz0.3 ~ 0.70.250.10.070.040.010.20.3
Titanium Ris ak Titanium alyaj ak konpozisyon chimik




KlasKonpozisyon chimik (fraksyon mas) (%) pa pi gran pase (eksepte pou valè ranje espesifye)
TibèkilalCrMouvmanSnMnVFesizoZrCNHOsòm lòt eleman yo
BT1-00Baz0.150.080.050.040.0080.10.1
BT1-0Baz0.250.10.070.040.010.20.3
BT1-2Baz1.50.150.10.150.010.30.3
OT4-0Baz0.4 ~ 1.40.5 ~ 1.30.30.120.30.10.050.0120.150.3
OT4-1Baz1.5 ~ 2.50.7 ~ 2.00.30.120.30.10.050.0120.150.3
OT4Baz3.5 ~ 5.00.8 ~ 2.00.30.120.30.10.050.0120.150.3
BT5Baz4.5 ~ 6.20.80.30.120.30.10.050.0150.20.3
BT5-1Baz4.3 ~ 6.02.0 ~ 3.00.30.120.30.10.050.0150.150.3
BT6Baz5.3 ~ 6.80.60.10.30.10.050.0150.20.3
BT6CBaz5.3 ~ 6.50.250.150.30.10.040.0150.150.3
BT3-1Baz5.5 ~ 7.00.8 ~ 2.02.0 ~ 3.00.2 ~ 0.70.15 ~ 0.040.50.10.050.0150.150.3
BT8Baz5.8 ~ 7.02.8 ~ 3.80.30.2 ~ 0.40.50.10.050.0150.150.3
BT9Baz5.8 ~ 7.02.8 ~ 3.80.250.2 ~ 0.351.0 ~ 2.00.10.050.0150.150.3
BT14Baz3.5 ~ 6.32.5 ~ 3.80.250.150.30.10.050.0150.150.3
BT20Baz5.5 ~ 7.00.5 ~ 2.00.250.151.5 ~ 2.50.10.050.0150.150.3
BT22Baz4.4 ~ 5.70.5 ~ 1.54.0 ~ 5.50.5 ~ 1.50.150.30.10.050.0150.180.3
Пt-7mBaz1.8 ~ 2.50.250.122.0 ~ 3.00.10.040.0060.150.3
Пt-3bBaz3.5 ~ 5.00.250.120.30.10.0400.150.3
AT3Baz2.0 ~ 3.50.2 ~ 0.50.2 ~ 0.50.2 ~ 0.40.10.050.0080.150.3

5. Ki aplikasyon ki nan plak la BT6 Titanium?

BT6 alyaj (Ti-6Al-4VL te jwenn yon aplikasyon lajè nan fabwikasyon an nan estrikti soude Titanium).

6. Avantaj nou yo

Nou Titanium alyaj fèy BT6 foto nan Baoji, objektif prensipal nou an se yo dwe yon fouisè pwofesyonèl nan fèy metal Titanium akBT6 Titanium plakak pri konpetitif ak pafè sèvis apre-sale nan kliyan nou yo. Nou konfòme yo ak chemen an nan devlopman pwofesyonèl ak genyen mache a ak nivo devlopman teknoloji dirijan nou yo ak bon jan kalite pwodwi ekselan.

7. Pake ak livrezon

Estanda pake ekspòtasyon: pake ka an bwa oswa anbalaj an bwa

10kg oswa anba a yo se carton oswa trip anbalaj

delivery and package baoji fairy titanium tmsalloy.com

Baj popilè: bt6 plak Titanium, Swèd, manifaktirè, faktori, pri, esansyèl, pou vann, nan stock, achte rabè